典型对比数据
(ODSi-RE0 替代日本协同 RE0)
检测项目 | 协同REO原样 | ODSi-RE0 |
锥入度(0次)25℃,0.1mm | 394 | 401 |
滴点,℃ | 201 | 228 |
铜片腐蚀(22h,100℃) | 4a | 1b |
蒸发量(22h,100℃),% | 1.09 | 0.42 |
四球较大无卡咬负荷 PB,N | 1254 | 1254 |
四球较压烧结负荷PD,N | 2450 | 2450 |
长磨(1200rpm,75℃,60min),mm | 0.4 | 0.39 |
长磨(1200rpm,75℃,240min),mm | 0.478 | 0.448 |
长磨(1200rpm,120℃,60min),mm | 0.467 | 0.384 |
长磨(1200rpm,120℃,240min),mm | 断线 | 0.504 |
低温转矩(-30℃),启动/运转,mN.m | 259/16 | 129/24 |
使用温度 | -30-120 | -30-120 |